Special-formula HDPE liner with enhanced OIT and HP-OIT retention for hot-climate containment, biogas lagoons, brine ponds and elevated-temperature wastewater service.
High-temperature resistant HDPE geomembrane is a special HDPE impermeable liner manufactured from virgin HDPE resin blended with high-performance composite antioxidant system and carbon-black UV stabilizer via extrusion-blowing process, complying with GRI-GM13 specification. Enhanced OIT & HP-OIT greatly improves anti-thermal-oxidative-aging performance under high-temperature service. Service condition: long-term medium temperature ≤60℃; short-term peak surface temperature up to 80-85℃ under solar exposure. Not suitable for continuous immersion above 65℃.
Swipe or scroll horizontally to view the complete table.
| Property | Unit | Minimum Requirement | Test Method |
|---|---|---|---|
| Density | g/cm³ | ≥0.940 | ASTM D1505 |
| Elongation at Yield | % | ≥12 | ASTM D6693 (Type IV) |
| Elongation at Break | % | ≥700 | ASTM D6693 (Type IV) |
| Carbon Black Content | % | 2.0-3.0 | ASTM D4218 / D1603 |
| Carbon Black Dispersion | Rating | Max Grade 3 | ASTM D5596 |
| Stress-Crack Resistance (SP-NCTL) | h | ≥500 | ASTM D5397 |
| Standard OIT | min | ≥120 | ASTM D3895 |
| High-Pressure OIT (HP-OIT) | min | ≥500 | ASTM D5885 |
| OIT retention after 85℃-90d thermal aging | % | ≥55 | ASTM D5885 |
| Property | Unit | 1.5 mm | 2.0 mm | 2.5 mm | 3.0 mm | Test Method |
|---|---|---|---|---|---|---|
| Tensile Yield Strength | kN/m | 22 | 29 | 37 | 44 | ASTM D6693 |
| Tensile Break Strength | kN/m | 40 | 53 | 67 | 80 | ASTM D6693 |
| Tear Resistance | N | 187 | 249 | 311 | 374 | ASTM D1004 |
| Puncture Resistance | N | 480 | 640 | 800 | 960 | ASTM D4833 |
Taiji supplies project-specific roll dimensions, surface options and formulation packages. Final selection should be confirmed against the operating environment, subgrade condition and installation plan.
High-temperature resistant HDPE geomembrane is special-formula HDPE liner complying with GRI-GM13. It adopts virgin HDPE resin plus high-efficiency composite antioxidant system and carbon-black UV stabilizer. Higher OIT & HP-OIT value improves anti-thermal-oxidative-aging performance under high-temperature working environment. Smooth, single-sided textured and double-sided textured are available.
Standard HDPE: OIT≥100 min, HP-OIT≥400 min, suitable for normal-temperature landfill, tailings ponds and common lagoons. High-temperature resistant HDPE: OIT≥120 min, HP-OIT≥500 min, with OIT retention ≥55 % after 85℃-90d thermal aging. It resists thermal-oxidative degradation better for hot manure lagoons, biogas ponds and salt evaporation ponds. Physical strength indexes are the same under equal thickness.
Yes. Single-sided textured and double-sided textured high-temperature resistant HDPE geomembrane can be produced by co-extrusion process. Texture asperity height ≥0.25 mm.
Main applications: livestock biogas lagoons, high-temperature manure lagoons, salt-field evaporation ponds, lithium-brine holding ponds, desert mining evaporation ponds, landfill leachate lagoons, hot-climate landfill capping and industrial hot-wastewater ponds. Long-term medium temperature shall not exceed 60 ℃.
No. Even with enhanced antioxidant formula, polyethylene substrate will suffer accelerated creep and aging under continuous immersion above 65 ℃. Short-term peak surface temperature up to 85 ℃ from solar radiation is acceptable.
Biogas fermentation will raise liquid temperature. High-temperature resistant grade is strongly recommended to slow down antioxidant consumption and extend service life. Standard HDPE will age faster under long-term fermentation heat.
Yes. Compatible with hot-wedge welder, extrusion welder and hot air gun. Welding parameters are similar to standard HDPE. Adjust temperature and speed according to site ambient condition. For textured grade, polish off texture bumps on overlap area before welding.
Yes. Geotextile cushion shall be laid above and below the liner to prevent puncture from sharp stones and debris.
Buried covered condition: over 30 years. For hot-liquid lagoons within 60 ℃ and exposed solar environment: 12-18 years, subject to actual operating temperature and site conditions.
Manufactured according to GRI-GM13 specification. Test reports including tensile, tear, puncture, OIT, HP-OIT and thermal-aging retention can be provided.
Common thickness:1.5 mm, 2.0 mm, 2.5 mm, 3.0 mm. Standard roll width:2-6 m. Smooth, single-sided textured and double-sided textured can be customized.